20130802
I have decided to use polyurethane varnish for the guitar.
First I pore fill using the wood pore filler.
Then I sand it level.
For the PU varnish I use wipe on technique to apply the varnish.
After each coat, I sand with 240 grit to level it.
After 3 coats, I still can't get a good shine.
I think I have wait for to to cure properly and meanwhile read more about applying PU varnish.
I probably need a few more coats.



Sanding the surface


Applying the pore filler


After 3 coats


Finishing the top. The surface felt smooth but not quite the shiny yet.


Close up of the finish


After 2 more coats and level sanded with 800 grit